- non shrinkage- no crack during curing
- low/high pressure injecting
- liquidity- tiny gap
- ready use pack
- high tensile strength
- high viscidity strength
- water-tight, durable, anti-corrosion of rebar
|
|
|
 |
| |
|
A : B = 2 :
1 (weight)
|
 |
 |
|
|
 |
| |
| 1. |
Pour hardener into resin. |
|
2. |
Mix thoroughly until light-brown color appearing. |
|
|
|
|
|
|
 |
| |
- remove all dirt, oil, grease from surface
by brushing or blowing
- locating the nipples distance between should
be equil to depth of crack。
- paste AE111 adhesive on nipples
- locating pin must be position in crack
- glue the nipple on concrete surface firmly
- seal all crack by AE111AB
- inject the mixed AE160AB into crack by high/low
pressure pumping system
- grinding off all sealing material and maintain
the surface smooth
|
|
|
 |
| |
- use up before pot-life.
- wear protect gloves.
- self life one year(15℃--25℃
storage).
- solvent to clean.
|
|
|
 |
| |
| density |
|
1~1.1kg/L
|
| operation
time |
20℃ |
120mins |
| viscosity |
20℃ |
400~500cps
|
| compressive
strength |
7days after |
600kg/c㎡ |
| tensile
strength |
7days after |
200kg/c㎡ |
| bending
strength |
7days after |
400kg/c㎡ |
| bonding
strength |
7days after |
120kg/c㎡
|
|
|